Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrason® S 3010 NAT - PSU - BASF

Material Data Center offers the following functions for Ultrason® S 3010 NAT:
unit conversion, PDF datasheet print, comparison with other plastics, parameters for material models, CAE Interfaces

Check here, which other Ultrason S datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Unreinforced, higher viscosity injection moulding and extrusion grade, tougher and with improved chemical resistance.
Abbreviated designation according to ISO 1043-1: PSU
Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 40 / * cm³/10min ISO 1133
Temperatura 360 / * °C -
Carga 10 / * kg -
Contracción posterior al moldeo, paralelo 0.7 / * % ISO 294-4, 2577
Contracción posterior al moldeo, normal 0.7 / * % ISO 294-4, 2577
ASTM Data
Contracción posterior al moldeo, paralelo 0.007 mm/mm ASTM D 955
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción - / 2550 MPa ISO 527
Esfuerzo de fluencia - / 75 MPa ISO 527
Alarg. en límite elástico - / 6 % ISO 527
Alarg. nominal a rotura - / >50 % ISO 527
Módulo de plastodeformación, 1h * / 2500 MPa ISO 899-1
Resistencia al impacto Charpy, +23°C - / N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C - / N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C - / 5.5 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C * / 6 kJ/m² ISO 179/1eA
ASTM Data
Esfuerzo de fluencia a tracción 80 / - MPa ASTM D 638
Alargamiento a la fluencia 5.7 / - % ASTM D 638
Módulo de flexión 2599 / - MPa ASTM D 790
Resistencia al impacto Izod con entalla, 1/8 in 10 / - J/m ASTM D 256
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temp. de transición vítrea, 10°C/min 187 / * °C ISO 11357-1/-2
Estabilidad al calor, 1.80 MPa 177 / * °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 183 / * °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 183 / * °C ISO 306
Coef.de expansión térmica lineal, paralelo 53 / * E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espesores de probeta 1.6 / * mm -
Yellow Card disponible sí / * - -
Combustibilidad a espesor h V-2 / * class IEC 60695-11-10
Espesores de probeta 3.0 / * mm -
Yellow Card disponible sí / * - -
Combustibilidad según índice de oxigeno 32.1 / * % ISO 4589-1/-2
ASTM Data
Estabilidad al calor @ 66 psi 182 °C ASTM D 648
Estabilidad al calor @ 264 psi 171 °C ASTM D 648
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz * / 3.1 - IEC 62631-2-1
Constante dieléctrica, 1MHz * / 3.1 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz * / 8 E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz * / 64 E-4 IEC 62631-2-1
Resistividad volumétrica específica * / >1E13 Ohm*m IEC 62631-3-1
Resistividad superficial específica * / >1E15 Ohm IEC 62631-3-2
Resistencia dieléctrica * / 37 kV/mm IEC 60243-1
Indice comparativo de linea de fuga * / 125 - IEC 60112
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de agua 0.8 / * % Sim. to ISO 62
Absorción de humedad 0.3 / * % Sim. to ISO 62
Densidad 1230 / - kg/m³ ISO 1183
Densidad 1240 kg/m³ ASTM D 792
Propiedades específicas del materialSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de viscosidad 72 / * cm³/g ISO 307, 1157, 1628
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 140 °C -
Tiempo de pre-secado 4 h -
Humedad de procesamiento ≤0.02 % -
Temperatura de la masa 330 - 390 °C -
Temperatura del molde 120 - 160 °C -
Funciones
Viscosidad-velocidad de cizallamiento , Ultrason® S 3010 NAT, PSU, BASF
Tensión de cizalla-velocidad de cizalla , Ultrason® S 3010 NAT, PSU, BASF
Esfuerzo-alargamiento , Ultrason® S 3010 NAT (Cond), PSU, BASF
Módulo secante-alargamiento , Ultrason® S 3010 NAT (Cond), PSU, BASF
Esfuerzo-alargamiento (isocrono) 23°C, Ultrason® S 3010 NAT (Cond), PSU, BASF
Módulo de plastodeformación-tiempo 23°C, Ultrason® S 3010 NAT (Cond), PSU, BASF
Curva de creep 23°C, Ultrason® S 3010 NAT (Cond), PSU, BASF
Volumen especifico-temperatura (pvT) , Ultrason® S 3010 NAT, PSU, BASF
Módulo a tensión-temperatura , Ultrason® S 3010 NAT (Cond), PSU, BASF
Fatigue strength , Ultrason® S 3010 NAT, PSU, BASF
Características
Procesamiento y forma de entrega
Moldeo por inyección, Extrusion del film, Extrusión de perfiles, Extrusión de láminas, Moldeo por soplado, Termoconformación
Forma de suministro
Sémola, Color natural
Disponibilidad regional
Demás información
Moldeo por inyección
PREPROCESSING
Pre/Post-processing, max. allowed water content: .02 %
Pre/Post-processing, Pre-drying, Temperature: 140 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 330 - 390 °C
injection molding, Melt temperature, recommended: 350 °C
injection molding, Mold temperature, range: 120 - 160 °C
injection molding, Mold temperature, recommended: 140 °C
injection molding, Dwell time, thermoplastics: 10 min

Pretreatment
Drying temperature: 130 - 150°C
Drying time: minimum 4h
recommended dryer: vaccum or dry air dryer
maximum moisture: 0,02 - 0,05%

Ultrason® can be injection molded by any type of machinery on the market, provided that the plasticizing unit and the mold temperature control system have been configured appropriately. The machinery manufacturer must be consulted if any doubts exist on the ability of various parts to withstand the high temperatures required (e.g. barrel, barrel head, bolted connections, etc.)

Long residence time in combination with high temperatures should be avoided e.g. by pump out material at regular intervals.
During extended interruptions, the barrel temperature should be lowered to about 250-280°C.

It has been found out that heating to the requested processing temperature and shutting down or lowering the temperature is best carried out in two steps.
First, the barrel temperatures are set at the lower processing temperature range for the particular thermoplastic (340 - 350 °C). As soon as these temperatures have reached a steady state, the material in the barrel is pumped out. Second, the barrel temperature can be set to the required processing temperature or the heaters can be shut down.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.